Most common mistakes that can lead to damages

· Temperature

Air and/or surface temperature are too high or too low.

· Humidity

Surface or air humidity is too high. Moisture seeping through the surface (e.g. blisters).

· Application damage

Pot life exceeded. Too much time between layers.

· Surface preparation

Lack of or wrong surface preparation for specific surfaces.

· Product quantity

Layers too thin or too thick.

· Mixing ratio

Wrong mixing ratio or thinning.

Damages due to humidity

Damages due to humidity

Damages due to humidity

Damages due to wrong product quantity

Inadequate cleaning

Lack of or wrong surface preparation

Wrong coating - lack of adhesion

Wrong coating - lack of adhesion